Data provided by DuPont Packaging Polymers. A transparent, exceptionally strong polyester film, coated on one side with an oxygen and moisture barrier PVDC copolymer. It is used as a substrate in combination with sealant webs, to produce a highly durable structure with excellent oxygen barrier. Can be printed with appropriate inks, including water based. The barrier coating may be adversely affected by certain solvents, if they are trapped during printing or laminating. |