Formolene® 4140T is a high melt flow homopolymer designed for injection and compounding usage requiring very high isotacticity. Its high crystallinity with added nucleation provides high flexural modulus along with optimal properties of tensile strength and elongation. These characteristics make it an excellent choice for applications in automotive, appliance and compounding markets.Information provided by Formosa Plastics Corporation, U.S.A. |