MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ex-Tech Plastics PerformaTech™ PVC XAS-11 Low Charging PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Engineered for packaging applications that contain non-ESD sensitive items to be transported within ESD controlled environments, PerformTech XAS-11 is a low charging (formerly known as anti-static) rigid vinyl or PET sheet designed for thermoforming

Characteristics:
Resists tribo-electric charge generation,
Produced in thickness of .010 to .060",
Engineered for packaging to contain non-ESD sensitive items to be transported within ESD controlled environments

End Uses:
Shipping trays
Clamshell packaging
Packaging where dust and dirt are issues
Products transported within a controlled environment

Information provided by Ex-Tech Plastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM D1505
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6300 psiASTM D882
Elongation at Break >= 100 %ASTM D882
Izod Impact, Notched 144 J/mSOP-MEC-002.01
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 143 °FASTM D648-96
 
Descriptive Properties
Cold Impact-35°CASTM D1790
Contact Corrosivityno corrosionFTM 101C
Gauge Tolerance+/-5%gamma or beta gauges
Polycarbonate Compatibilityno attackEIA 564
Tribocharging<0.13 nC/in2Bellcore GR1421-CORE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEXTEC994 / 133219

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.