MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nexeo® HIVAL® 2435 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Features:
  • Food Contact Acceptable
  • Good Dimensional Stability
  • Good Processability
  • Good Surface Finish
  • Homopolymer
Uses:
  • Caps
  • Closures
  • Containers
  • Household Goods
  • Sporting Goods
  • Thin-walled Parts
  • Toys
Agency Ratings: FDA 21 CFR 177.1520RoHS Compliance: RoHS CompliantForms: PelletsProcessing Method: Injection Molding

Information provided by Nexeo® Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.904 g/ccASTM D792
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4600 psiASTM D638
Flexural Modulus 170000 psiASTM D790
Izod Impact, Notched 0.600 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 203 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 430 °F
Middle Barrel Temperature 450 °F
Front Barrel Temperature 470 °F
Nozzle Temperature 470 °F
Melt Temperature 470 °F
Mold Temperature 70.0 - 120 °F
Injection Pressure 400 - 1500 psi
Back Pressure 150 - 500 psi
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow

PNEXEO907 / 197591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.