MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Bonding Agent 2005 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Bonding Agent 2005 is a high performance, reactive and phthalate-free one-component bonding agent used to improve the adhesion of PVC plastisol coatings to substrates made of polyester or polyamide. It has low viscosity and therefore easy to handle during processing. Bonding Agent 2005 is a formulation in n-butyl acetate.

Chemical composition: Formulation of an aromatic polyisocyanurate in n-butyl acetate

Supply form: Lightly yellow

CAS Reg. No.: 123-86-4 (n-butyl acetate)

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccDIN 51 757
Viscosity 65 - 105 cPDIN EN ISO 3219/A.3
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature <=40.0 °C
 
Descriptive Properties
Content<0.2%Monomer (TD), DIN 55956
 40 percentActive
 6.3-6.7%NCO, DIN EN ISO 11909, app. A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8460 / 208853

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.