MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

PoolKemie SILIMOLD BLD-26 RTV2 silicon moulding rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Introduction: It is a two component room temperature vulcanizing pourable fluid silicon which cures on the addition of the appropriate CATALYST B*, according to the polycondensation process. A highly anti-adherent flexible compound, that is extremely accurate in its reproduction of fine details.

Application: SILIMOLD BLD-26 silicon rubber is ideal in the manufacture of moulds for the shoe industry (production of master moulds for rubber soles), technical items in general, and decorative plaster subjects like ceiling roses, frames, and wherever the reproduction of undercuts is not requested, due to its moderate tearing resistance.

Note 1: Tests have been carried out under these conditions: Temperature: +20°C; After: 24 ore; R.H.: 60%; Catalysis: 100:5

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 - 1.33 g/cc1.23 - 1.33 g/ccBefore Catalysis
Viscosity 2000 - 3000 cP2000 - 3000 cPBefore Catalysis
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inafter 5 days ageing, After Catalysis; ISO 4823
Storage Temperature 5.00 - 30.0 °C41.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 22 - 2822 - 28After Catalysis; DIN 53505
Tensile Strength 15.5 - 16.5 MPa2250 - 2390 psiAfter Catalysis; DIN 53504 - S A 3
Elongation at Break 230 - 270 %230 - 270 %After Catalysis; DIN 53504 - S A 3
Tear Strength 4.50 - 5.50 kN/m25.7 - 31.4 pliAfter Catalysis; ASTM D 624 S A 3
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hourDemoulding time
Pot Life 50.0 - 60.0 min50.0 - 60.0 minwith Catalyst B, See note 1, During Catalysis
Shelf Life 12.0 Month12.0 MonthBoth components (A and B) in their original tightly closed containers, in a dry and cool place , away from moisture
 
Descriptive Properties
AppearanceFlexible rubberAfter Catalysis
 Thick LiquidBefore Catalysis
ColorGreenComponent B, Before Catalysis
 Light GreyComponent A, Before Catalysis
 Semi bright light greenAfter Catalysis
Mixing ratio100:5by weight, Before Catalysis
Pouring Time50 minSee note 1, During Catalysis

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOOLK009 / 318488

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.