MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Fluon® FC 423 PTFE, 15% Graphite Powder Fiber Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Fluon® FC 423 (340 423 010) is a 15% graphite powder-filled PTFE product designed for use in seal applications. This compound is supplied in round pelletized form. These pellets range in size from approximately 350 – 800 microns.

End Uses: Graphite powder is added to PTFE to improve the lubricity and wear properties of PTFE especially against soft metals.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.11 g/ccASTM D4745
Bulk Density 0.650 g/ccASTM D4894
Filler Content 15 %ASTM D4745
Linear Mold Shrinkage 0.022 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58Sustained; ASTM D2240
 61Peak; ASTM D2240
Tensile Strength 1900 psiASTM D4745
Elongation at Break 120 %ASTM D4745

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
AGC Fluon® FC123 PTFE, 15% Graphite Filled
AGC FC 123 PTFE, 15% Graphite
AGC FC 423 PTFE, 15% Graphite
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder

PAGCX095 / 191204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.