MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo Technyl® A 246M Nylon 66, Impact Grade, EH50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.

Technyl A 246m offers an excellent notched impact resistance at low temperatures making it suitable for sports and leisure applications. It is suitable for shoe soles, ski components, ski and surf bindings, as well as toy applications, such as the bumper of a remote-controlled car.

This product is available in natural, white and black.

Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183-A
Water Absorption 1.05 %(Beginning Dry) 24 hours in water 23°C. ISO 62
Linear Mold Shrinkage 0.019 cm/cmRHODIA-EP
Linear Mold Shrinkage, Transverse 0.019 cm/cmRHODIA-EP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 35.0 MPaISO 527
Tensile Strength, Yield 42.0 MPaISO 527
Elongation at Break 210 %ISO 527
Elongation at Yield 210 %ISO 527
Tensile Modulus 0.600 GPaISO 527
Flexural Yield Strength 27.0 MPaISO 178
Flexural Modulus 0.700 GPaISO 178
Izod Impact Resistance 8.00 J/cm²ISO 180
Charpy Impact Unnotched NBISO 179/EU-1993
Charpy Impact, Notched 10.0 J/cm²ISO 179/1EA-1993
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 ohm-cmIEC 93
Surface Resistance 1.00e+13 ohmIEC 93
Dielectric Constant 4.0
@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 38.0 kV/mmIEC 243-1
Dissipation Factor 0.060
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 3146-C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 270 °C
Middle Barrel Temperature 260 - 280 °C
Front Barrel Temperature 270 - 290 °C
Melt Temperature 518 - 554 °F
Mold Temperature 140 - 194 °FSurface
Drying Temperature 176 °FDehumidifying Dryer
Dry Time 3 - 4 hour
Moisture Content <= 0.20 %
Back Pressure 50.0 - 100 psi
Fill Speed 300 - 600 mm/secPeripheral Screw Speed
 
Descriptive Properties
Injection Speed (cm3/sec)80 - 150 cm3/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® ST801 NC010A PA66-HI
Delrin Delrin® 100P NC010 POM
Domo Technyl® A 246M Nylon 66, Impact Grade, EH0
Plastcom SLOVAMID 66 MI LS PA66, improved strength
Celanese Hostaform® C 2521 POM, Unfilled

PRHO09 / 65942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.