Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical properties including transparency and glossiness, and making the material ideal for further processing. Transparency:Superior transparency and glossiness even for applications involving processing of thick objects. Ease of Processing: Excellent fluidity and melt tension characteristics suited to a wide range of molding methods. - Inflation molding - can be molded into even thick or wide products with superior bubble stability.
- Extrusion lamination - can be drawn down even at high speed.
- Blow molding - can be molded producing a very smooth surface.
- Injection molding - can be molded even into very thin products.
Strength: Good balance in length and breadth with superior tearing strength lengthways. Application: Extrusion lamination Features: Drawing down ability Information provided by UBE. |