MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wieland Simidur Superior PFM Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Material Notes: Palladium-base ceramic alloy

Applications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials

Dental

Key Words: EN ISO 9693
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.7 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 200HV5/30; after porcelain firing
 230HV5/30; hardened
Tensile Strength, Yield 54960 psi
@Strain 0.2 %
after porcelain firing
 75350 psi
@Strain 0.2 %
hardened
Elongation at Break 17 %hardened
 34 %after porcelain firing
Modulus of Elasticity 113 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.5 µm/m-°C
@Temperature 25.0 - 500 °C
Melting Point 2210 - 2350 °F
Solidus 2210 °F
Liquidus 2350 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1560 °FPreheating Temp.
Casting Temperature 2550 °F
 
Component Elements PropertiesOriginal ValueComments
Silver, Ag 23.4 %
 
Descriptive Properties
Colorwhite

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Palladium Alloy
Overview of materials for Refractory Metal
Niobium FS-85 (Nb-28Ta-10W-1Zr), Recrystallized
Niobium C-103 (WC 103; 89Nb-10Hf-1Ti), Cold-Rolled
NAECO® ELKONIUM® 43 palladium based alloy

NWIELAN18 / 19820

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.