MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® HTNFR42G30NH NC010 PA-GF30FR(40)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes:

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 138 MPaDAM; ISO 527-1/-2
Elongation at Break 1.8 %DAM; ISO 527-1/-2
Tensile Modulus 10600 MPaDAM; ISO 527-1/-2
Flexural Strength 216 MPaDAM; ISO 178
Flexural Modulus 11200 MPaDAM; ISO 178
Charpy Impact Unnotched 46.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VDAM; IEC 60112
 >= 600 V
@Thickness 3.00 mm
DAM; UL 746A
 
Thermal PropertiesOriginal ValueComments
Melting Point 315 °Cfirst heat; ISO 11357-1/-3
UL RTI, Electrical 130 °C
@Thickness 0.400 mm
UL 746B
 130 °C
@Thickness 1.50 mm
UL 746B
 130 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 0.400 mm
UL 746B
 115 °C
@Thickness 1.50 mm
UL 746B
 120 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 0.400 mm
UL 746B
 125 °C
@Thickness 1.50 mm
DAM; UL 746B
 130 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 0.400 mm
DAM; IEC 60695-11-10
Glow Wire Ignition Temperature 750 °C
@Thickness 0.400 mm
DAM; IEC 60695-2-12
 800 °C
@Thickness 1.50 mm
DAM; IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
DAM; IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.400 mm
DAM; IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
DAM; IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
DAM; IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature >= 325 °CInjection; -
 <= 335 °CInjection; -
Mold Temperature >= 110 °CInjection; -
 <= 130 °CInjection; -
Drying Temperature 100 °C
@Time 21600 - 28800 sec
Dehumidified Dryer; Injection Molding; Injection
Moisture Content 0.10 %Injection
 
Descriptive Properties
AdditiveRelease agent
Delivery formPellets
Part Marking Code>PPA-GF30FR<SAE J1344
 PA-GF30FR(40)ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA-GF30FR(40)ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
RTP Company RTP 4005 FR  Polyphthalamide (PPA) Glass Fiber 30% - Flame Retardant
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement

PDSY5448s / 239851

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.