MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil 832 Mobil DTE 800 Series
Categories: Fluid; Lubricant

Material Notes: Mobil DTE 832 and 846 are superior performance turbine oils designed for use in steam turbines, gas turbines and combined cycle gas turbine (CCGT) applications under the most severe operating conditions. These progressive products are based on high quality hydrotreated basestocks for exceptional thermal/oxidation resistance along with specially chosen additives engineered to provide the deposit control and "keep-clean" performance required by severe duty gas turbines as well as excellent water separability needed for steam turbine operation. The formulations also include a non-zinc antiwear system to meet the load carrying requirements of geared turbines. In addition to meeting the separate requirements of modern steam and gas turbine designs, Mobil DTE 800 Series are excellent choices for combined cycle applications that require a single oil for a gas turbine and a steam turbine run in tandem. Simultaneously meeting both deposit control and water separation requirements is the key performance highlight of this advanced lubricant technology. The excellent thermal/oxidative resistance of Mobil DTE 832 and 846 ensures that they can be operated in the most severe turbine environments. The performance features of Mobil DTE 800 Series oils translate into excellent equipment protection, reliable operation, with reduced down-time and extended oil charge life. These products also provide the ultimate flexibility to the operator because they can be used in all turbine types: steam, gas and geared-turbines.

Mobil DTE 832 and 846 are superior performance turbine oils designed for use in steam and gas turbine oil systems, direct- or gear-coupled and turbine speed control mechanisms. Specific applications include: Combined cycle (CCGT) electric power generation applications including those with a common circulation system for the steam turbine and gas turbine; Lubrication of steam turbine or gas turbine units used for electric power generation, natural gas pipeline transmission, process operations and cogeneration plants

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.860 g/cc
@Temperature 15.6 °C
ASTM D4052
Viscosity Measurement 110Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 29.6 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.4 cStASTM D445
Oxidative Stability 1200 hourRotating Bomb Oxidation Test (RBOT); ASTM D2272
 >= 10000 hourTurbine Oil Stability Test (TOST); ASTM D943
 
Thermal PropertiesOriginal ValueComments
Pour Point -30.0 °CASTM D97
Flash Point 224 °CASTM D92
 
Descriptive Properties
Air Release, ASTM D3427, minutes2@ 50°C
Copper Strip Corrosion1A3 hrs @ 100°C
Demulsibility Time (min)15to 3 mL emulsion @ 54°C
Foam Sequence I, ASTM D97020/0
Foam Sequence II, ASTM D89320/0
Foam Sequence III, ASTM D89320/0
FZG Scuffing, DIN 5182, A/8.3/90, Fail Stage9
Rust Prevention, Distilled WaterpassASTM D665A
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON150 / 75575

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.