MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ensinger TECACOMP PA6 ID blue 1053686 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes:
  • detectable via metal detector
  • x-ray detectable
  • Explanation of food contact according to
  • FDA and EU 10/2011 on request
  • high toughness
  • resistant to many oils, greases and fuels
Target Industries:
  • food technology

Information provided by Ensinger Inc.

Vendors: Ensinger TECACOMP compounds withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm0.020 in/inDIN EN ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psiDIN EN ISO 527-1
Elongation at Break 20 %20 %DIN EN ISO 527-1
Modulus of Elasticity 2.70 GPa392 ksiDIN EN ISO 527-1
Charpy Impact Unnotched 15.8 J/cm²75.2 ft-lb/in²DIN EN ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDIN 53765
Maximum Service Temperature, Air 100 °C212 °Flong term
 150 °C302 °Fshort term
Glass Transition Temp, Tg 5.00 °C41.0 °Fmoist; DIN 53765
 60.0 °C140 °Fdry; DIN 53765
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 300 °C500 - 572 °F
Mold Temperature 70.0 - 110 °C158 - 230 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
 
Descriptive Properties
Colorblue
Detectability2.3 mm Al4 x 4 x 4 mm, metal detectable
 2.4 mm Al4 x 4 x 4 mm, x-ray detectable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9010 / 318938

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.