MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 9864DU TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; very good hydrolysis and microbial resistance; very good low-temperature impact strength; opaque; Cylindrical pellets; Application; Boot shells; Technical parts

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 98ISO 868
Hardness, Shore D 61ISO 868
Tensile Strength, Ultimate 7980 psi200 mm/min; DIN 53504
Elongation at Break 420 %200 mm/min; DIN 53504
Tensile Modulus 220 MPa
@Temperature 60.0 °C
storage; ISO 6721-1,-4
 610 MPa
@Temperature 20.0 °C
storage; ISO 6721-1,-4
 1280 MPa
@Temperature -20.0 °C
storage; ISO 6721-1,-4
50% Modulus 0.0200 GPa
@Strain 50 %
200 mm/min; DIN 53504
100% Modulus 0.0240 GPa
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 0.0370 GPa
@Strain 200 %
200 mm/min; DIN 53504
Flexural Modulus 310 MPa2 mm/min; ISO 178
Rebound 55 %Resilience; ISO 4662
Tear Strength 140 kN/m500 mm/min; ISO 34-1
Abrasion 28mm3; ISO 4649 method A
Compression Set 46 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 47 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 265 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 110 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 9868DU Polyurethane
Covestro Desmopan® 3378A TPU
Covestro Desmopan® 3856D TPU
Covestro Desmopan® 9855DU TPU
Covestro Desmopan® 9852DU TPU

PCOVEST0728 / 202511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.