MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ganpati Exim SKN-18 NBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: The Nitrilast rubber is a product of low temperature co-polymerization of butadiene with a CAN, using an emulsifier – tail of potassing soap or mixture of soaps on the rosin and fatty acids. The vulcanizate of Nitrilast differs from its analogues by higher physico-mechanical figures and by higher benzene and oil resistance. The vulcanizate, extended by Nitrilast, considerably exceed abrasion resistance of NR. The grades of this rubber as Nitrilast 18, 18M have also a great coo-resistance. The rubber can be mixed with polyvinylchlorvinyl resin, phenolformaldehyde, acrylonitrilestyrene and other resins that may be used also as peptizer agents.

Application: The Nitrilast rubber is applied for manufacturing a variety of benzene and oil resistant goods for auto, aircraft and rubber technical industries.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 80 - 120
@Temperature 100 °C
80 - 120
@Temperature 212 °F
ML (1+4), Group1
Ash <= 0.60 %<= 0.60 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength <= 18.6 MPa<= 2700 psi
Elongation at Break <= 450 %<= 450 %
 
Descriptive Properties
Content<0.4%Organic acid soaps
 <4.5%Organic acid
 0.5-1.2%Antioxidant, Agidol-2
 1.0-1.5%Antioxidant, VS-30A
 17-20%Bound Nitrile of acrylic acids
Mass losses at drying0.008

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI024 / 317308

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.