MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper, UNS C61900, HR10 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Spring and Stress Relieved

Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding, Capacity for Being Hot Formed; Good Suitability – Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Soldering, Brazing, Capacity for Being Cold Worked

Common Fabrication Processes: Bending; Blanking; Forming; Shearing; Stamping

Typical uses: Contacts; Springs; Switch Components; Marine Hardware

Applicable Specifications: Bar – ASTM B124/B124M, ASTM B150/B150M; Die – Forgings ASTM B283/B283M; Electrode – Welding MILITARY MIL-E-23765/3; Forgings, Die (Hot Pressed) – ASME SB283; Rod – ASTM B124/B124M; Rod, Bar & Shapes - Aluminum Bronze ASME SB150, Aluminum Bronze ASTM B150/B150M; Shapes – ASTM B150/B150M, ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.50 g/cc0.271 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1050 MPa
@Thickness 1.02 mm
152000 psi
@Thickness 0.0400 in
Tensile Strength, Yield 1000 MPa
@Thickness 1.02 mm
145000 psi
@Thickness 0.0400 in
0.2% Offset
Elongation at Break 1.0 %
@Thickness 1.02 mm
1.0 %
@Thickness 0.0400 in
Tensile Modulus 110 GPa16000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000164 ohm-cm0.0000164 ohm-cm10.5% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.418 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 6.61 W/m-K45.9 BTU-in/hr-ft²-°F
Melting Point 1041 - 1050 °C1905 - 1920 °F
Solidus 1041 °C1905 °F
Liquidus 1050 °C1920 °F
Annealing Point 538 - 788 °C1000 - 1450 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 549 - 827 °C1020 - 1520 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.5 - 10 %8.5 - 10 %
Copper, Cu 84.1 - 88.5 %84.1 - 88.5 %As Balance
Iron, Fe 3.0 - 4.5 %3.0 - 4.5 %
Lead, Pb <= 0.020 %<= 0.020 %
Tin, Sn <= 0.60 %<= 0.60 %
Zinc, Zn <= 0.80 %<= 0.80 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC61900x4 / 293028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.