  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Angst+Pfister APSOplast® PEEK EC Conductive PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: This PEEK is reinforced with carbon fibre and is electrically and thermally conductive. It can be used for applications where problems can arise due to discharge on parts which come into contact with people. This material is also ideally suited for holding or fixing devices used for the conveyance of silicon wafers in production processes or for the manufacture of sensitive electronic components including hard disks and PCBs.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³DIN EN ISO 1183-1
Water Absorption  0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
DIN EN ISO 62
 0.030 %
@Time 346000 sec
0.030 %
@Time 96.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 253 MPa36700 psiDIN EN ISO 2039-1
Tensile Strength at Break 106 MPa15400 psi50 mm/min; DIN EN ISO 527
Tensile Strength, Yield 106 MPa15400 psiDIN EN ISO 527
Elongation at Break 4.0 %4.0 %DIN EN ISO 527
Elongation at Yield 4.0 %4.0 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 4.70 GPa682 ksiflexural test; DIN EN ISO 178
 4.80 GPa696 ksitensile test; DIN EN ISO 527
Flexural Strength 178 MPa25800 psiDIN EN ISO 178
Compressive Strength  27.0 MPa
@Strain 1 %,
Load 1.02 kg
3920 psi
@Strain 1 %,
Load 2.25 lb
5 mm/min; EN ISO 604
 47.0 MPa
@Strain 2 %,
Load 1.02 kg
6820 psi
@Strain 2 %,
Load 2.25 lb
5 mm/min; EN ISO 604
Compressive Modulus 3.60 GPa522 ksiEN ISO 604
Charpy Impact Unnotched 5.80 J/cm²27.6 ft-lb/in²DIN EN ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm - 1e+051000 ohm-cm - 1e+05DIN EN 61340-2-3
Surface Resistance 100 - 10000 ohm100 - 10000 ohmDIN EN 61340-2-3
 
Thermal PropertiesMetricEnglishComments
CTE, linear  50.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 140 °F
 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 0.460 W/m-K3.19 BTU-in/hr-ft²-°F
Melting Point 341 °C646 °FISO 11357-3
Maximum Service Temperature, Air 260 °C500 °Flong term
 300 °C572 °Fshort term
Glass Transition Temp, Tg 147 °C297 °FDIN 53765
Flammability, UL94 V-0V-0
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP065 / 250563

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.