MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic protection, it was observed during processing to have exceptional hot workability. ATI 425™ titanium is an alpha-beta alloy that utilizes iron in place of some higher-cost vanadium as a beta stabilizer.

Information provided by ATI Wah Chang

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.162 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 32 - 36
Tensile Strength, Ultimate 146000 psiLong.
 159000 psiTrans.
Tensile Strength, Yield 129000 psiLong.
 152000 psiTrans.
Elongation at Break 13 %Trans.
 14 %Long.
Modulus of Elasticity 119 GPaLong.
 143 GPaTrans.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000154 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1600 - 1650 °C
Solidus 1600 °C
Liquidus 1650 °C
Beta Transus 957 - 971 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.0 %
Iron, Fe 1.5 %
O2 0.25 %
Titanium, Ti 91.75 %
Vanadium, V 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate
Iron Aluminide, FeAl
ATI Allvac® 38-644 UNS R58640 Titanium Alloy
MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite
Molybdenum Disilicide, MoSi2

NATIWC08 / 15063

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.