MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ensinger TECACOMP PA66 CF40 black 1014832 Nylon 66, 40% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Carbon Fiber Filled

Material Notes:
  • very high stiffness
  • good wear properties
  • good heat deflection temperature
  • resistant to many oils, greases and fuels
  • good weldable and bondable
  • low viscosity

Information provided by Ensinger Inc.

Vendors: Ensinger TECACOMP compounds withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.32 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 262 MPaDIN EN ISO 527-1
Elongation at Break 1.8 %DIN EN ISO 527-1
Modulus of Elasticity 26.8 GPaDIN EN ISO 527-1
Charpy Impact Unnotched 47.0 kJ/m²DIN EN ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 ohm-cmDIN EN ISO 3915
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDIN 53765
Maximum Service Temperature, Air 110 °Clong term
 170 °Cshort term
Glass Transition Temp, Tg 5.00 °Cmoist; DIN 53765
 72.0 °Cdry; DIN 53765
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 310 °C
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 - 120 °C
Dry Time 4.00 - 8.00 hour
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO9016 / 318944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.