MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® LLDPE 318BJ PE (Asia)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE 318BJ is a butene linear low density polyethylene resin typically designed for easy processing and specially formulated for optimum thermal stability at high temperatures used in cast film extrusion. Cast film produced from SABIC® LLDPE 318BJ exhibit excellent optical properties, puncture resistance and tear strength .SABIC® LLDPE 318BJ is TNPP free. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 2.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.0 MPa1890 psiProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
Film Elongation at Break, MD 470 %470 %Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
Film Elongation at Break, TD 600 %600 %Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
Puncture Energy 57.0 J42.0 ft-lbJ/m; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; SABIC method
Elmendorf Tear Strength MD 65 g65 gProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D1922
Elmendorf Tear Strength TD 300 g300 gProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D1922
Dart Drop Test 75.0 g0.165 lbProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D1709
Film Tensile Strength at Break, MD 28.0 MPa4060 psiProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
Film Tensile Strength at Break, TD 18.0 MPa2610 psiProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
1% Secant Modulus, MD 135 MPa19600 psiProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
1% Secant Modulus, TD 140 MPa20300 psiProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 98.0 °C208 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 5.0 %
@Thickness 0.0300 mm
5.0 %
@Thickness 0.00118 in
2.5 BUR using 100% 318BJ.; ASTM D1003
Gloss 90 %90 %60°; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11057 / 244524

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.