MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrofol® DE 1-4 000000 Polycarbonate
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Characterization: Makrofol DE 1-4 000000 is an extrusion film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol DE 1-4 000000 comprises all of the well known advantages of polycarbonate, such as excellent mechanical and optical properties. Makrofol DE 1-4 000000 maintains accurate graphic registration regardless of the forming method due to low internal stress. Cost savings relative to gloss/gloss films are realized using this product as no masking is supplied in Makrofol DE 1-4 000000 ’s standard configuration. Typical applications are automotive, labels, membrane switches, nameplates, and medical packaging. Makrofol DE 1-4 000000 is available in various standard thicknesses from 0.005 ” to 0.030 ” (125 microns to 750 microns). Other thicknesses are available on request. The surface combination of Makrofol DE 1-4 000000 is one side gloss and one side fine matte for printability. As with any product, use of Makrofol DE 1-4 000000 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.33 %
@Time 86400 sec
immersion; ASTM D570
Water Absorption at Saturation 0.20 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 72.4 MPaASTM D882
Tensile Strength, Yield 62.7 psiASTM D882
Elongation at Break 125 %ASTM D882
Flexural Modulus 330000 psiASTM D790
Tear Strength 1100 pliASTM D1004
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 - 120 °C
DIN 53752
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 - 120 °C
DIN 53752
Flammability, UL94 V-2
Shrinkage >= 0.40 %
@Temperature 130 °C,
Time 3600 sec
parallel; IEC 53752
 >= 0.40 %
@Temperature 130 °C,
Time 3600 sec
across; IEC 53752
 
Optical PropertiesOriginal ValueComments
Gloss <= 9.0 %60° reverse side; ISO 2813
 >= 90 %60° top side black inked second surface; ASTM D2457
Yellow Index 1.0 %ASTM E313
Transmission, Visible >= 70 %>20 mil; ASTM D1003
 >= 80 %<20 mil; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrofol® DE 1-1 000000 Polycarbonate
Covestro Makrofol® DE 6-2 Polycarbonate
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® DE 7-2 Polycarbonate
Covestro Makrofol® ID 4-4 Polycarbonate

PB09868 / 92708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.