MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Wacker Semicosil® 970 TC A/B Conductive Adhesive Sealant
Categories: Polymer; Thermoset; Silicone; Silicone Elastomer, for Thermal Management

Material Notes: SEMICOSIL® 970 TC A/B is a pasty, but still flowable addition-curing, two component elastomeric silicone that cures at elevated temperature to an thermally conductive silicone rubber.

Special features:

  • two-component
  • thermal conductivity
  • pasty, still flowable
  • almost constant properties between -40 °C and +180 °C
  • primerless adhesion
Application:
  • versatile interface material for heat sink applications for the electronics industry
  • thermally conductive adhesive material
  • applicable as thin interface layer between PCB and metal housings of electric control units
  • heat ablation in lighting modules

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.26 g/ccComponent A
 2.26 g/ccComponent B
 2.26 g/cccured; DIN 53479 A/ISO 2781
Viscosity 25000 cP
@Shear Rate 10.0 1/s
Component A, plate-paste-rotational viscosimeter
 30000 cP
@Shear Rate 10.0 1/s
Catalyzed A+B
 35000 cP
@Shear Rate 10.0 1/s
Component B, plate-paste-rotational viscosimeter
 85000 cP
@Shear Rate 0.500 1/s
Component A, plate-paste-rotational viscosimeter
 94000 cP
@Shear Rate 0.500 1/s
Catalyzed A+B
 120000 cP
@Shear Rate 0.500 1/s
Component B, plate-paste-rotational viscosimeter
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65DIN 53505/ISO 868
Tensile Strength at Break 4.00 MPa
Elongation at Break 90 %
Tear Strength 7.00 kN/m
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.800 W/m-K
 
Processing PropertiesOriginal ValueComments
Pot Life 960 minCatalyzed A+B
 
Descriptive Properties
Appearancewhite-grayCatalyzed A+B
 white-grayComponent A
 white-grayComponent B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials TSE3280G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials TSE3282-G Thermally Conductive Silicone Adhesive
Momentive Performance Materials TSE3281G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials TSE3281G Adhesive Sealant, Thermally Conductive
Master Bond Mastersil 705TC One Component, Thermally Conductive Silicone

PWACK9424 / 204953

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.