MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
ITW Densit® WEARSPRAY 2000 Ceramic Lining
Categories: Ceramic; Oxide

Material Notes: Densit® WearSpray 2000 wear resistant linings provide excellent protection against moderate wear at temperatures up to 400°C (750°F).

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 21.9 lb/galEN 1015-6
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity <= 60.0 GPaDynamic; 70
Flexural Strength 12.0 MPaEN 196-1
Compressive Strength 110 MPaEN 12190
Abrasion 1.0 - 1.5cm3/50cm2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
Specific Heat Capacity 0.900 - 1.00 J/g-°C
Thermal Conductivity 1.50 W/m-K
Maximum Service Temperature, Air 750 °F
 
Component Elements PropertiesOriginal ValueComments
Al2O3 + TiO2 50 %EN 196-10
CaO 13 %EN 196-10
Fe2O3 <= 0.20 %EN 196-10
SiO2 35 %EN 196-10
 
Descriptive Properties
Chromate, Cr6+ Content (%)<0.0002EN 196-10
Erosive Resistance (min/cm3)100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWDE9087 / 239597

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.