MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTARIN® C MG POM/Medical Grade Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes:
  • Good combination of rigidity, stiffness and toughness
  • Multi-sterilizable with hot steam, plasma as well as ethylene oxide
  • Low moisture absorption
Product applications:
  • Mechanical engineering
  • Pharmaceutical industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ASTM D792
Water Absorption 0.90 %0.90 %ASTM D570
 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888ASTM D785
Hardness, Rockwell R 120120ASTM D785
Hardness, Shore D 8585ASTM D2240
Tensile Strength, Yield 65.5 MPa9500 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Tensile Modulus 2.76 GPa400 ksiASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.210.21
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+16 ohm1.00e+16 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 99.0 µm/m-°C55.0 µin/in-°FASTM D696
Thermal Conductivity 0.231 W/m-K1.60 BTU-in/hr-ft²-°F
Melting Point 166 °C330 °F
Maximum Service Temperature, Air 82.2 °C180 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C225 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Zelux® 20% GF Polycarbonate
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled
Röchling SUSTARIN® H POM/Acetal Homopolymer
Röchling SUSTARIN® C POM/Acetal Copolymer
LG Chemical LUPOY GP1000L PC, Transparent

PROCH9031 / 232734

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.