Product Description: Affinity PL 1881G R Polyolefin Plastomer (POP) is produced via INSITE Technology. It is designed for a variety of demanding packaging applications, including high-speed, form-fill-seal products. - Excellent ultimate hot tack strength
- Low temperature sealability
- Ability to seal through contamination
- Outstanding optics
Complies with: US FDA FCN 424; HPFB No Objection (with limitations); EU, No 10/2011; ISCC Plus certification for renewable-based plastics. Consult the regulations for complete details.Availability: Asia Pacific; Europe; Latin America; North America Additive: Antiblock: 2500 ppm; Slip: 750 ppm Agency Ratings: EU No 10/2011; FDA FCN 424; HPFB (Canada) No Objection; ISCC PLUS Form: Pellets Processing Method: Blown Film Information provided by The Dow Chemical Company |