MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ A-43 Bonding Agent, Primer and Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties:
  • Adhesion promoter for most thermoplastics, thermoset materials, elastomers, polyurethanes.
  • Can be used on metals, glass and ceramic

Applications: High functionality produces good bond strength in bonding difficult-to-bond substrates, such as polyethylene. Suitable for a wide range of vulcanizing elastomers as adhesion promoter to most substrates for a wide range of vulcanizing elastomers. Used as a primer for PU and TPU overmolding to a wide range of substrates. Higher bond strengths with less material use, but lower moisture resistance than A-3. Ambient cure 60 min or short thermal cure. Slight amber.

Key Words: Epoxy Adhesive, Sealant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.018 - 1.038 g/ccASTM D1298
Viscosity Measurement 4.5 - 8.5ASTM D445
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.442 - 1.448ASTM D1218
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 - 60.0 minAmbient
 5.00 min
@Temperature 150 °C
 15.0 min
@Temperature 75.0 °C
 
Descriptive Properties
ColorClear with stray color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BACT DLC Diamond-Like Coating
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)
Kuraray SEPTON® S76 Soft Compound
Covestro Texin® 260 Thermoplastic Polyurethanes (TPU)
Covestro Desmopan® 460 Thermoplastic Polyurethane

PAQREL00 / 24216

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.