This product is part of a range of Heat Curable Inks designed specifically for use in Photovoltaic panels. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has excellent adhesion, chemical and environmental resistance properties. Excellent adhesion to glass Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester, mesh 156 to 325tpi Substrate: GlassInformation provided by Gwent Electronic Materials Ltd. |