MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Kostat 7440 Conductive ABS Compound
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD injection molded products.

Special Features

This product exhibits high conductivity, easy processing, smooth sheet surface, and tight dimensional tolerances after injection molding. This makes KOSTAT 7440 suitable for various injection molding applications.

Applications:

KOSTAT 7440 is recommended for electronics packaging such as ESD Trays and other injection molded products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Linear Mold Shrinkage 0.0067 cm/cm0.0067 in/in
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7575ASTM D785
Tensile Strength, Yield 55.0 MPa7980 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Strength 65.0 MPa9430 psiASTM D790
Flexural Modulus 5.47 GPa793 ksiASTM D790
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm10000 ohm-cmKostat Rv
Surface Resistivity per Square 1e+051e+05Kostat Rs
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 188 °C340 - 370 °F
Middle Barrel Temperature 188 - 210 °C370 - 410 °F
Front Barrel Temperature 210 - 232 °C410 - 450 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese CoolPoly® D3608 Thermally Conductive High Temperature Polyamide (HTN)
Celanese Coolpoly® D3606 Thermally Conductive Polyamide 4,6
Celanese Coolpoly® D1202 Thermally Conductive Polypropylene

PKOSTAT24 / 49059

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.