MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ME-2570B Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2500 series are super high flow, high density, high performance thermoplastic elastomer designed for demanding exterior automotive applications, including window encapsulation. Sarlink ME-2570B is a medium hardness, high density injection molding grade excellent UV resistance and adhesion to glass with primer.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion Good Flexibility; Good Processability; Good Surface Finish; Good Toughness; High Density; High Flow; High Specific Gravity; Medium Hardness; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183
Viscosity 123 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 5.00 sec
ISO 868
 74
@Time 1.00 sec
ISO 868
Tensile Strength at Break 856 psiFlow; ISO 37
 943 psiAcross Flow, 20 mm/mm; ISO 37
 839 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Change in Air; ISO 188
 1060 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain 305 psi
@Strain 100 %
Across Flow, 20 mm/mm; ISO 37
 334 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 730 %Flow; ISO 37
 800 %Across Flow, 20 mm/mm; ISO 37
 815 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Change in Air; ISO 188
 896 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
Tear Strength 160 pliFlow; ISO 34-1
 160 pliAcross Flow, Method Ba, Angle (Unnicked; ISO 34-1
Compression Set 22 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 46 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 76 %
@Temperature 90.0 °C,
Time 252000 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 338 - 374 °F
Middle Barrel Temperature 347 - 383 °F
Front Barrel Temperature 356 - 401 °F
Nozzle Temperature 356 - 401 °F
Melt Temperature 356 - 401 °F
Mold Temperature 59.0 - 104 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1081 / 237572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.