MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik TEGO® Antifoam MR 1015 Antifoam concentrate
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam MR 1015 is a 70 % active antifoam concentrate based on modified siloxanes.

Application: TEGO® Antifoam MR 1015 is used as an antifoam in a broad range of aqueous based systems. It is particularly recommended for metal working fluids (MWF) and textile auxiliaries. Applications for TEGO® Antifoam MR 1015 are:

  • textile industry (e. g. textile bleaching, dying, finishing, production of non-wovens)
  • in metal working fluids (pre-defoamer in concentrates and for tank-side addition)
  • other industrial applications (e. g. industrial and household cleaners)
Properties / Benefits: Due to the special modification and formulation of the active material, TEGO® Antifoam MR 1015 combines excellent efficiency with maximum compatibility at the same time. The result is a unique product profile which cannot be achieved either with organic or with traditional silicone oil based antifoams. Furthermore, undesirable effects associated with silicone oil based antifoams (silicone spotting, fish eyes) can be eliminated in most applications. TEGO® Antifoam MR 1015 shows excellent alkaline and electrolyte stability, even at higher temperatures. In addition TEGO® Antifoam MR 1015 is easily water dispersible, which allows for easy handling.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
 
Descriptive Properties
Appearancemilky, turbid
Content70%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik SIPERNAT® 383 DS Silica Powder
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® D 13 Silica Powder
Evonik SIPERNAT® D 10 Ceramic Powder
Evonik SIPERNAT® 50 Silica Powder

PEVONIL556 / 196760

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.