MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Poco Graphite SUPERSiC® Basic Silicon Carbide
Categories: Ceramic; Carbide

Material Notes: The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for specific applications.
POCO’s unique conversion process produces the highest quality silicon carbide products available on the market today. This process starts with graphite material specially designed and manufactured for use as the precursor in the conversion process. Near net parts are machined in graphite, purified, and subjected to a proprietary conversion process which substitutes pure silicon atoms for carbon atoms. The result is SUPERSIC, POCO’s high purity silicon carbide.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.53 g/cc
Apparent Bulk Density 3.13 g/cc
Open Porosity 19 %
Porosity 20 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 1992[kg/mm2]
Tensile Strength, Yield 129 MPa
Modulus of Elasticity 216 GPa
Flexural Strength 155 MPa
Compressive Strength 110 MPa
Poissons Ratio 0.17
Fracture Toughness 2.30 MPa-m½
Shear Modulus 96.0 GPaDynamic
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.400 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.40 µm/m-°Cat RT
Thermal Conductivity 170 W/m-K
 
Descriptive Properties
Specific stiffness85 5N.m/g
Total Impurity Level (ppm), Max10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-650/42 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
SGL Carbon Group EK 20 Carbon Graphite
Corning Eagle XG® Slim Display Glass

CPOCO33 / 85610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.