MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Semicosil® 925 Silicone Gel
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: SEMICOSIL® 925 is a high purity, one-component addition curing RTV-2 silicone gel.

Special features:

  • Low ion content
  • Low volatile content
  • Low viscosity
  • Good mechanical damping properties
Application: SEMICOSIL® 925 is a dielectric gel especially designed to seal, protect and preserve the electrical characteristics of delicate electronic components (e.g. bonded chips on hybrid components which are exposed to extreme external influences).

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/cc
Solids Content 100 %
Brookfield Viscosity 700 cP
 
Mechanical PropertiesOriginal ValueComments
Penetration 10
@Load 0.100 kg
[mm]
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Constant 2.5
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 21.7 kV/mmIEC 60243
Dissipation Factor 0.00010
@Frequency 1000 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -65.0 °CASTM D2137
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
@Treatment Temp. 120 °C
 3.00 min
@Treatment Temp. 150 °C
 35.0 min
@Treatment Temp. 100 °C
 
Descriptive Properties
AppearanceTransparent liquid
Content<1 ppmExtractable Ion Content K
 <3 ppmExtractable Ion Content Na
 <5 ppmExtractable Ion Content Cl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SMAC SMACWRAP® ST Damping Material, 1 mm
Wacker Elastosil® R 401/10 Silicone Rubber
SMAC SMACMOUNT® 2528S 02 Damping Material
SMAC SMACFOAM® 1250S-01 Damping Material
SMAC BARRIER® Damping Material

PWACK9416 / 204945

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.