MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Telles Mirel™ F3002 Thermoforming Grade PHA Bioplastic  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: Mirel F3002 thermoforming food contact grade is suitable for a wide range of thermoformed food service and packaging applications including cold and hot cups, cup lids, yogurt containers, tubs and trays for meats and vegetables, condiment cups, other single-serve and disposable food packaging. The material is suitable for storage as well as food service, from frozen food storage and microwave reheating to boiling water up to 212°F.

About Mirel Bioplastics

Mirel is a family of bioplastic materials that have physical properties comparable to petroleum-based resins, yet are both biobased and biodegradable in natural soil and water environments, home composting systems, and industrial composting facilities, where these facilities are available. The rate and extent of Mirel's biodegradablility will depend on the size and shape of the articles made from it. However, like nearly all bioplastics and organic matter, Mirel is not designed to biodegrade in conventional landfills.

Telles is a joint venture between Metabolix and Archer Daniels Midland Company.

Key Words: Polyhydroxyalkanoate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Oxygen Transmission 10.2 cc-mm/m²-24hr-atm26.0 cc-mil/100 in²-24hr-atmASTM D3985
Viscosity 1700 cP
@Temperature 180 °C
1700 cP
@Temperature 356 °F
Apparent Melt Viscosity, per 100 sec; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 13 %13 %ASTM D638
Flexural Modulus 1.48 GPa215 ksiASTM D790 A
Izod Impact, Notched 0.370 J/cm0.693 ft-lb/inASTM D256 A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C241 °FASTM D648 B
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FASTM D648 B
Vicat Softening Point 136 °C277 °FASTM 1525 A10
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 175 °C347 °FReverse Temperature Profile
Middle Barrel Temperature 170 °C338 °F
Front Barrel Temperature 165 °C329 °F
Die Temperature 165 °C329 °FCenter Zone
 165 °C329 °FEdge Zones
Melt Temperature 165 - 170 °C329 - 338 °F
Roll Temperature <= 32.0 °C<= 89.6 °FA-roll (Top roll of a down-stack)
 50.0 - 65.0 °C122 - 149 °FB-roll (Middle roll)
 65.0 °C149 °FC-roll (Bottom roll of a down-stack)
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Equipment recommendation: Screw Profile<3Low compression ratio. Any mixing sections should be low shear design.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Telles Mirel™ F1005 Injection Molding Grade PHA Bioplastic
Telles Mirel™ I6003rp Biobased PHA Polymeric Modifier
Telles Mirel™ F1006 Injection Molding Grade PHA Bioplastic

PMETAA990 / 108487

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.