MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® Polyspeed® G-R92-GIL-R92 Epoxy -Glass Fiber Laminate
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Polyspeed® G-R92-GIL-R92 is an unidirectional epoxy laminate with a thin glass fiber fabric in the mid-position. The laminate is supplied in roll form. Widths are available from 38 - 1200 mm.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 935 - 1265 MPa136000 - 183500 psiValue 0°; EN ISO 527
Tensile Modulus 33.1 - 44.9 GPa4800 - 6510 ksiValue 0°; EN ISO 527
Tear Strength 0.1122 - 0.1518 kN/m0.6402 - 0.8662 pliValue 0°; EN ISO 527
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 125 °C257 °F
 
Descriptive Properties
Content24-30%Resin
Glass Fiber Reinforcement1748-1932 g/m2Areal Weight
 2400 texGlass Fiber Roving
 28.5-31.5 g/m2Glass Fiber Fabric

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9303 / 322459

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.