MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NYCOA 534H PA 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: high viscosity, heat stabilized, nucleated nylon for tubing, sheet, film and molding

Information provided by NYCOA, Inc.

Key Words: PA 6, Polyamide 6, Nylon 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
Water Absorption 1.8 %1.8 %ASTM D570
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength, Yield 83.0 MPa12000 psiASTM D638
Elongation at Break >= 130 %>= 130 %ASTM D638
Flexural Yield Strength 114 MPa16500 psiASTM D790
Flexural Modulus 2.689 GPa390.0 ksiASTM D790
Izod Impact, Notched 0.590 J/cm1.11 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D789
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 °C482 °F
Rear Barrel Temperature 220 °C428 °F
Middle Barrel Temperature 230 °C446 °F
Front Barrel Temperature 250 °C482 °F
Nozzle Temperature 250 °C482 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 76.0 °C169 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NYCOA 2084 HS PA 6
NYCOA 715C PA 6
NYCOA 2084 HS Super-Tough, High Viscosity Nylon 6 Resin
NYCOA 400 PA 6
NYCOA 436 PA 6

PNYCOA31 / 55577

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.