MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DIAB Rigid Foam IPN 20-649 Type 1  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset

Material Notes: This material was primarily developed for insulation of liquid H2 fuel tanks for launch vehicles. The material, which is referred to as an Inter-Polymer-Network, consists of a polymeric alloy of a highly cross-linked polyamide-urea and a ductile linear vinyl polymer. The cryogenic properties are good and the material exhibits excellent short-term capability at high temperatures. IPN 20-649 us thermo-formable.

Information provided by DIAB, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0397 - 0.0500 g/cc0.00144 - 0.00181 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 0.689 - 1.00 MPa100 - 145 psiat 296 K; in Plane
 0.900 MPa131 psiat 20K
Elongation at Break 1.5 %1.5 %at 20K
 5.0 %5.0 %at 296 K; in Plane
 10 %10 %at 296 K; Shear Strain; all directions
Tensile Modulus 0.0200 - 0.0300 GPa2.90 - 4.35 ksiat 296K; in Plane
Compressive Strength 0.500 - 0.6998 MPa72.5 - 101.5 psiat 296 K; Through Plane
Compressive Modulus 0.0200 GPa2.90 ksiat 296 K; Through Plane; ASTM D1621-A
 0.0500 GPa7.25 ksiat 296 K; Through Plane; ASTM D1621-B
Poissons Ratio 0.300.30
Shear Modulus 0.0120 - 0.01700 GPa1.74 - 2.465 ksiat 296K; all directions
Shear Strength 0.400 - 0.600 MPa58.0 - 87.0 psiat 296 K; all directions
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature -183 - 37.0 °C
22.2 µin/in-°F
@Temperature -297 - 98.6 °F
Thermal Conductivity 0.0150 W/m-K0.104 BTU-in/hr-ft²-°F100K
 0.0270 W/m-K0.187 BTU-in/hr-ft²-°F210K
 0.0330 W/m-K0.229 BTU-in/hr-ft²-°F310K

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam
Armacell ArmaFORM® FR100 PET foam core
DuPont Mobility and Materials Vespel® SF-0920 Polyimide Foam, Low Density
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
ITW Insulation TRYMER® Supercel Phenolic Insulation 2.5 lb/ft³ Density

PDIAB66 / 29837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.