Product Description: Riteflex RKX-150 is an unfilled Thermoplastic Polyester Elastomer with a Shore D hardness of 40. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Material Status: Experimental Information provided by Celanese |