MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ovako 46MnVS3 SB9850 Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: 46MnVS3 is a micro-alloyed steel suitable for forging where no further heat-treatment is necessary. SB9850 is treated to give excellent machinability. Two available variants are SB9850 and 382K.

Information provided by Ovako

Key Words: SB9850 - S620*, 1.1305
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 235 - 270
@Thickness 15.0 - 23.0 mm
Round bar
 235 - 270
@Thickness 24.0 - 30.0 mm
Round bar
 235 - 270
@Thickness 31.0 - 50.0 mm
Round bar
 235 - 270
@Thickness 51.0 - 90.0 mm
Round bar
Tensile Strength 775 - 890 MPa
@Thickness 15.0 - 23.0 mm
Round bar
 775 - 890 MPa
@Thickness 24.0 - 30.0 mm
Round bar
 775 - 890 MPa
@Thickness 31.0 - 50.0 mm
Round bar
 775 - 890 MPa
@Thickness 51.0 - 90.0 mm
Round bar
Tensile Strength, Yield >= 540 MPa
@Thickness 51.0 - 90.0 mm
Rel, Round bar
 >= 560 MPa
@Thickness 31.0 - 50.0 mm
Rel, Round bar
 >= 580 MPa
@Thickness 24.0 - 30.0 mm
Rel, Round bar
 >= 620 MPa
@Thickness 15.0 - 23.0 mm
Rel, Round bar
Elongation at Break 16 %
@Thickness 24.0 - 30.0 mm
Round bar
 16 %
@Thickness 31.0 - 50.0 mm
Round bar
 16 %
@Thickness 51.0 - 90.0 mm
Round bar
 18 %
@Thickness 15.0 - 23.0 mm
Round bar
Reduction of Area 35 %
@Thickness 15.0 - 23.0 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 314 °CMS
 733 °CAC1
 794 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.030 %
Carbon, C 0.42 - 0.46 %
Chromium, Cr <= 0.30 %
Iron, Fe 97.61 - 98.68 %As Balance
Manganese, Mn 0.70 - 1.0 %
Molybdenum, Mo <= 0.080 %
Nitrogen, N 0.0090 - 0.020 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.40 %
Sulfur, S 0.040 - 0.060 %
Titanium, Ti <= 0.010 %
 
Descriptive Properties
WeldabilityCEV 0.65max
 Pcm 0.55max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NOVAKO315 / 234614

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.