MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips OSP™ System OSP510R EMCM Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Ethylene Methyl Acrylate Cyclohexene Methyl Acrylate (EMCM) is a polymer that will oxidize but not degrade. CHMA content 14.0% (wt.). Primary antioxidant 150 ppm. Oxygen capacity 65 cc/gm.

OSP510R is designed for use in coextruded cast film and coating applications at gauges of 0.25 mil to 1.5 mil of a non-food contact layer. This resin should be blended with one of the Catalyst/Photoinitiator Masterbatches in order to properly activate the oxygen scavenging mechanism. Typical blend ratios range from 95:5 to 85:15 (EMCM/MB) with 90:10 being the recommended blend ratio for most applications. Recommended extrusion melt temperatures range from 250°F to 400°F when blended with OSP100M Masterbatch. Higher melt temperature extrusion of up to 550°F is possible when blending with OSP150M.

OSP polymers are used in packaging for O2-sensitive applications from food to electronics. Packaging produced with OSP polymers can extend product life, eliminating waste and providing greater distribution flexibility. Oxygen scavenging rates and capacities are influenced significantly by UV activation dose, use conditions such as storage temperatures, and initial package oxygen content.

Information provided by Chevron Phillips Chemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³
Melt Flow 6.5 g/10 min6.5 g/10 min
 
Processing PropertiesMetricEnglishComments
Melt Temperature 121 - 288 °C250 - 550 °FDepends on masterbatch

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips OSP™ System OSP520R EMCM Resin

PCHEVOSP01 / 20334

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.