MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ TF 2072Z PTFE Fine Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Dyneon™ TF 2072 Z PTFE is an ideal grade for thin-wall, small diameter tubing and wire and cable insulations, processed by paste extrusion method at reduction ratio up to 3000:1. This product offers more economic processing because of larger usable preforms.

Product Features:

  • High molecular weight
  • Needs less lubricant than TF 2071 Z (1-2 parts by weight)
  • Emulsion polymerization PTFE
  • Product grade with lower extrusion pressure than TF 2071 Z
  • Meets ASTM D4895-04 Type 1, Grade 1, Class C classification
  • Processing by standard paste extrusion methods

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.470 g/cc0.0170 lb/in³DIN EN ISO 60
Density 2.17 g/cc0.0784 lb/in³DIN EN ISO 12086
Particle Size 440 µm440 µmaverage; ISO 13320
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiDIN EN ISO 527-3
Elongation at Break 470 %470 %DIN EN ISO 527-3
 
Descriptive Properties
Extrusion Pressure40 MPareduction ratio 400:1, ASTM D4895
Reduction Ratio Range50-3000:1Dyneon Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ TFM™ 1700 PTFE
3M Dyneon™ TF 2071USZ PTFE
3M Dyneon™ TF 2053Z PTFE Fine Powder
3M Dyneon™ TF 2029Z PTFE Fine Powder
3M Dyneon™ TF 2025Z PTFE Fine Powder

PDYNE044a / 149083

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.