MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ISONATE™ 125M Pure MDI
Categories: Fluid

Material Notes: ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers for polyurethane processing. Judicious use of polyols, extenders and additives permits the manufacture of thermoplastic polymers suitable for extrusion, injection molding or solution applications.

98% 4,4`-diphenylmethane diisocyanate and 2% 2,4`-diphenylmethane diisocyanate

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/cc
Viscosity 5.0 cP
@Temperature 43.0 °C
Vapor Pressure <= 0.000100 torr
@Temperature 43.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.0030% as HCl
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 136 J/g
Heat of Vaporization 360 J/g
CTE, linear 762 µm/m-°C
@Temperature 20.0 °C
volumetric
Specific Heat Capacity 1.80 J/g-°C
Thermal Conductivity 0.000300 cal cm/sec-cm²-°C
Boiling Point 314 °C
Decomposition Temperature 230 °C
Flash Point >= 177 °CClosed Cup; ASTM D93
 
Processing PropertiesOriginal ValueComments
Shelf Life 1.50 Month(45 days) at 43°C, clear melt without filtration
 12.0 Monthat -20°C, clear melt without filtration
 
Descriptive Properties
Hydrolyzable Chloride ppm18
Isocyanate Equivalent Weight125.5
NCO Content wt%33.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ISONATE™ 50 O,P` Pure MDI
3M K37 Glass Bubbles
3M S38HS Glass Bubbles
3M S38 Glass Bubbles
Celanese 50000445 Methyl Isobutyl Carbinol (MIBC)

PDOW1388 / 30606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.