MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Materion E20 Beryllium/BeO Composite, 20 Volume% BeO  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Beryllium Alloy

Material Notes: Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic properties. This mix is hot isostatically pressed (HIP'd) into fully dense blocks for further processing into finished blanks and subsequent machining into components.

These materials are used in electronic packaging heat sinks for MCM-L, SEM-E, BGA's, and RF/Microwave applications. The CTE can be controlled by varying the BeO content to match with die materials like GaAs or silicon in RF/microwave applications or match AuSn or AuGe over brazing/soldering temperatures, Kovar, Alloy 46 or 48, and other packaging materials.

Can be machined by conventional processes. Corrosion resistance similar to aluminum. For protection in severe environments such as salt fog, the composite may be coated in a number of ways such as electroless or electrolytic nickel plating, chrome plating, and gold or silver plating for brazing or soldering operations.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

Information provided by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 2.05 g/cc>= 0.0739 lb/in³
 2.06 g/cc0.0744 lb/in³Average
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity >= 301 GPa>= 43700 ksi
 303 GPa43900 ksiTypical
Fracture Toughness 13.7 MPa-m½12.5 ksi-in½Average KIC.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.50 - 11.0 µm/m-°C
@Temperature 25.0 - 100 °C
5.28 - 6.11 µin/in-°F
@Temperature 77.0 - 212 °F
 11.5 µm/m-°C
@Temperature 25.0 - 250 °C
6.39 µin/in-°F
@Temperature 77.0 - 482 °F
average
Specific Heat Capacity 1.584 J/g-°C0.3786 BTU/lb-°F
Thermal Conductivity >= 200 W/m-K>= 1390 BTU-in/hr-ft²-°F
 210 W/m-K1460 BTU-in/hr-ft²-°FTypical
 
Component Elements PropertiesMetricEnglishComments
BeO 25.8 - 32.25 %25.8 - 32.25 %
Beryllium, Be 79.37 - 83.5 %79.37 - 83.5 %As remainder; includes Be from BeO
Oxygen, O 16.5 - 20.63 %16.5 - 20.63 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO
Materion Thermalox® 995 General Purpose 99.5% BeO
Beryllium I-220H Grade 1

NBBC00 / 15310

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.