MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Traid Villarroya TVH® TV 2017-T3 (AA 2017) Aluminum alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes:
  • High mechanical properties
  • Great resistance to fatigue
Industry Applications:
  • Screws
  • Bolts
  • High structural resistance components for aviation industry
  • Defense

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.85 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 135135
Tensile Strength at Break 470 MPa68200 psiRm
Tensile Strength, Yield 390 MPa56600 psiRp 0.2
Elongation at Break 11 %11 %
Modulus of Elasticity 75.0 GPa10900 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000051 ohm-cm0.0000051 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.6 µm/m-°C13.1 µin/in-°F
Thermal Conductivity 134 W/m-K930 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.65 - 95.5 %91.65 - 95.5 %As Remainder
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 3.5 - 4.5 %3.5 - 4.5 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.40 - 1.0 %0.40 - 1.0 %
Manganese, Mn 0.40 - 1.0 %0.40 - 1.0 %
Silicon, Si 0.20 - 0.80 %0.20 - 0.80 %
Zinc, Zn <= 0.25 %<= 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NTRAID940a / 318920

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.