MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Matexcel MCP-015 Ordered Mesoporous Carbon
Categories: Other Engineering Material

Material Notes: Mesoporous carbon is a new type of non-silicon-based mesoporous material with huge specific surface area (up to 2500m2/g) and pore volume (up to 2.25cm3/g), which is very promising in catalyst supports, hydrogen storage materials, electrodes. Materials and other aspects have been important applications, so they are highly valued by people. In addition, the charge storage of the electric double layer capacitor material made of the mesoporous material is higher than that of the assembled metal oxide particles, and is much higher than that of the commercially available metal oxide electric double layer capacitor.

Morphology: Powder

Key Words: Synonyms: Ordered Mesoporous Carbon
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product overviewPore size (nm): 3.8~4.0 Specific surface area (m²/g): 900~1200 Total pore volume (cm3/g): 0.9~1.3 Micropore volume(cm3/g): 0.18 Microporosity (%): 3.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK2032 / 300663

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.