MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Low warpage

Application: E&E item

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0090 cm/cm0.0030 - 0.0090 in/inASTM D955
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 250 °C
11 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9191ASTM D785
Tensile Strength, Yield 123 MPa
@Thickness 3.20 mm
17800 psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break 5.0 %
@Thickness 3.20 mm
5.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Strength 181 MPa
@Thickness 3.20 mm
26300 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 8.04 GPa
@Thickness 3.20 mm
1170 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 0.686 J/cm
@Thickness 6.40 mm
1.29 ft-lb/in
@Thickness 0.252 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
@Thickness 6.40 mm
410 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
@Thickness 6.40 mm
392 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 75.0 °C167 °FUL 746B
UL RTI, Mechanical with Impact 75.0 °C167 °FUL 746B
UL RTI, Mechanical without Impact 75.0 °C167 °FUL 746B
Flammability, UL94 HB
@Thickness 0.720 mm
HB
@Thickness 0.0283 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 255 °C464 - 491 °F
Middle Barrel Temperature 245 - 255 °C473 - 491 °F
Front Barrel Temperature 250 - 260 °C482 - 500 °F
Nozzle Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 245 - 260 °C473 - 500 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 120 °C
@Time 14400 - 18000 sec
248 °F
@Time 4.00 - 5.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00254 - 0.00381 cm0.00100 - 0.00150 in
 
Descriptive Properties
Ram Speed SettingMedium to Fast
Screw SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
Avient Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT)
Celanese Crastin® SK605 BK851 PBT-GF30
Celanese Crastin® LW9030 BK851 PBT+ASA-GF30
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity

PLBA10 / 50367

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.