MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R plus 4305/50 batch Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R plus 4305/50 HCR silicone rubbers are addition-curing, two part compounds (batch grades). The vulcanizates show excellent transparency and good to very good mechanical properties. Properly postcured vulcanizates of ELASTOSIL® R plus 4305/50 comply with BfR and FDA food contact regulations. The material also passes USP XXIII Class VI and ISO 10993 certification is available.

Application: ELASTOSIL® R plus 4305/50 is intended for fabrication of extruded articles that afford high transparency and very good tear resistance values.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 - 1.14 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM D2240
Tensile Strength at Break 11.5 MPaASTM D412
Elongation at Break 850 %ASTM D412
Tear Strength 40.0 kN/mASTM D624
Compression Set 15 %
@Temperature 175 °C,
Time 79200 sec
WSTM 1114
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
post cured 4h/200°C
Pot Life 1440 minWSTM 2299
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9285 / 204814

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.