MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wefapress PETP-SP with Solid Lubricant
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: PETP-SP is a polyethylene terephthalate modified with solid lubricants. This composition leads to "self-lubrication" of the material, to improve the sliding properties and wear resistance of the material compared to pure PETP. This promotes greater carrying capacity and also prevents the slip-stick effect.

Information provided by Wefapress.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 128 MPa
@Time 30.0 sec
18600 psi
@Time 0.00833 hour
DIN ISO 2039 Teil 1
Tensile Strength 65.0 MPa9430 psiDIN 53455
Tensile Strength, Ultimate 75.0 MPa10900 psiDIN 53455
Elongation at Break 5.0 %5.0 %DIN ISO / R 527
Modulus of Elasticity 2.20 GPa319 ksiDIN 53457
1% Secant Modulus 1.00 MPa145 psiEU 1935/2004 - EU 10/2011 (FSP Quality)
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²DIN 53457
Coefficient of Friction 0.200.20
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FDIN ISO 11359
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°F
Melting Point 255 °C491 °FDTA
Maximum Service Temperature, Air 75.0 °C167 °FDimensional Stability; DIN 53461
 100 °C212 °FContinuous Application Temp.
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEFA938 / 243143

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.