MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals Novapol® LF-0224-A LDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Puncture value is 43.2 J/mm. LDPE. Excellent stiffness, moderate toughness, easy processability. Additive Package: Base Resin.

Applications: Industrial packaging, liners, blends with LLDPE, foam articles.

Film properties are typical of 38 µm blown film extruded at a blow-up ratio of 2.5:1, but depend on operating conditions.

Information supplied by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D792
Thickness 38.1 microns1.50 mil
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.2 MPa1620 psiASTM D882
Film Tensile Strength at Yield, TD 12.0 MPa1740 psiASTM D882
Film Elongation at Break, MD 186 %186 %ASTM D882
Film Elongation at Break, TD 513 %513 %ASTM D882
Secant Modulus, MD 0.193 GPa28.0 ksiASTM D882
Secant Modulus, TD 0.258 GPa37.4 ksiASTM D882
Coefficient of Friction >= 0.60>= 0.60ASTM D1894
Elmendorf Tear Strength, MD 10.5 g/micron267 g/milASTM D1922
Elmendorf Tear Strength, TD 3.90 g/micron99.1 g/milASTM D1922
Dart Drop 2.40 g/micron61.0 g/milF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 27.2 MPa3950 psiASTM D882
Film Tensile Strength at Break, TD 17.8 MPa2580 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 9.9 %9.9 %ASTM D1003
Gloss 49.3 %49.3 %at 45°; ASTM D 2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FA6220 Low Density Polyethylene
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin

PEHM47 / 35509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.