HumiSeal® Stripper 1100 removes dual cure acrylated urethane conformal coatings such as UV40 family products. HumiSeal® Stripper 1100 does not contain any halogenated hydrocarbons, aromatics or flammable ingredients. Unlike methylene chloride based products that evaporated quickly, HumiSeal® Stripper 1100 remains on the surface to penetrate and soften the coating. HumiSeal® Stripper 1100 will not remove or attack solder, copper, silver, gold and nickel plating. HumiSeal® Stripper 1100 is in full compliance with the RoHS Directive (Directive 2002/95/EC).Information provided by Chase Electronic Coatings. |