MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese VECTRA A625 LCP, 25% Graphite Filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Solid Lubricant Filled

Material Notes: Good wear characteristics. 25% graphite filled.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183
Moisture Absorption 0.0300 %0.0300 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6262ISO 2039-2
Tensile Strength at Break 140 MPa20300 psi5mm/min; ISO 527-2/1A
Elongation at Break 5.7 %5.7 %5mm/min; ISO 527-2/1A
Tensile Modulus 9.00 GPa1310 ksi50mm/min; ISO 527-2/1A
Flexural Strength 140 MPa20300 psiISO 178
Flexural Modulus 10.5 GPa1520 ksiISO 178
Compressive Strength 56.0 MPa
@Strain 1 %
8120 psi
@Strain 1 %
ISO 604
Compressive Modulus 9.00 GPa1310 ksiISO 604
Izod Impact, Notched (ISO) 22.0 kJ/m²10.5 ft-lb/in²ISO 180/1A
 62.0 kJ/m²
@Temperature 23.0 °C
29.5 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 6.70 J/cm²31.9 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179/1eA
Tensile Creep Modulus, 1 hour 9800 MPa1.42e+6 psiISO 899-1
Tensile Creep Modulus, 1000 hours 7500 MPa1.09e+6 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Constant  13
@Frequency 1e+6 Hz
13
@Frequency 1e+6 Hz
IEC 60250
 30
@Frequency 100 Hz
30
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.040
@Frequency 100 Hz
0.040
@Frequency 100 Hz
IEC 60250
 0.15
@Frequency 1e+6 Hz
0.15
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 9.00 µm/m-°C5.00 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-2
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 114 °C237 °FISO 75-1, -2
Vicat Softening Point 159 °C318 °FISO 306
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 285 - 295 °C545 - 563 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 270 - 280 °C518 - 536 °F
Zone 2 275 - 285 °C527 - 545 °F
Zone 3 280 - 290 °C536 - 554 °F
Zone 4 285 - 295 °C545 - 563 °F
Die Temperature 290 - 300 °C554 - 572 °F
Melt Temperature 285 - 295 °C545 - 563 °F
 293 °C559 °FISO 294
Mold Temperature 60.0 °C140 °FISO 294
Injection Velocity 150 mm/sec5.91 in/secISO 294
Drying Temperature >= 150 °C>= 302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 48.0 MPa6960 psiISO 294
 50.0 - 150 MPa7250 - 21800 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  80 rpm
@Diameter 40.0 mm
80 rpm
@Diameter 1.57 in
 140 rpm
@Diameter 25.0 mm
140 rpm
@Diameter 0.984 in
 200 rpm
@Diameter 16.0 mm
200 rpm
@Diameter 0.630 in
 
Descriptive Properties
Injection moldingYes
Injection speedvery fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Vectra® A422 Liquid Crystal Polymer (LCP), Glass/Graphite Filled
Celanese Zytel® 151L NC010 PA612
Celanese VECTRA A130 LCP, 30% Glass Reinforced
Celanese VECTRA S625 LCP, 25% Specialty
Celanese VECTRA® 2355MT Carbon Fiber Reinforced Liquid Crystal Polymer (LCP)

PHCQ491 / 178946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.